Case Studies: Solving Pressure Distribution Problems

A manufacturer and supplier of load cells and torque and pressure sensors solved fluctuations in clamping pressure during manufacture in part through the use of a pressure-recording film.

The clamping pressure used to bond Futek’s metal foil strain gage to the transducer body was not initially uniform. Source: Sensor Products Inc.


Futek (Irvine, CA), manufacturer and supplier of load cells and torque and pressure sensors, experienced difficulty assembling some of its load cells to specification. By performing several tests, and controlling different variables, the company found fluctuations in clamping pressure to be a significant factor.

Futek’s sensors incorporate metal foil strain gage technology. The adhesive the company uses to bond the gages to sensors requires a clamping pressure of 50 to 75 psi. However, by using Pressurex from Sensor Products Inc. (Madison, NJ) Futek was able to see that the pressure fluctuated from 50 psi to upwards of 200 psi in some of its production runs.

Pressurex is a thin flexible film that easily and rapidly shows inconsistencies in surface pressure between mating and contacting surfaces.

This discovery led Futek to use Pressurex to help redesign several of its clamps to incorporate silicone die springs to regulate the pressure more precisely. “A sample pack of Pressurex with film that revealed different surface pressure ranges allowed our production to continue,” says James Meiselbach, a mechanical engineer at Futek.

Pressurex reveals surface pressure from 2 to 43,200 psi. No training or instrumentation is required. It is ideal to assess surface contact inconsistencies in virtually any industrial or electronic application, including gaskets, clamps, bolted joints, connectors, heat sinks, heat sealing elements, welding heads, and plastic and composite manufacture.

Meiselbach found using Pressurex to be a simple procedure. To measure the surface pressure of a clamp around the outside of a load cell, he cut Pressurex in the configuration of the clamp surface area, placed it in between the clamp and the load cell, applied force, unclamped it, and removed the Pressurex. He then compared the film, which changes color depending on how much pressure is exerted, to an accompanying color calibration chart.

Meiselbach became aware of Pressurex while working for an aerospace company. “We were having a problem with the main rotor blade of a helicopter. Interference was causing a fatigue crack in one of the inner spar tubes of the rotor blade,” says Meiselbach. “We put a large sheet of Pressurex in the bonding tool, bagged it up and pressurized it in the autoclave. When we removed the film, we were able to identify the exact amount of pressure causing the crack.”
    Sensor Products Inc.
    (973) 884-1755
    www.sensorprod.com


Benefits

  • Pressurex film allowed Futek to see that pressure fluctuated from 50 psi to upwards of 200 psi in some of its production runs.

  • This discovery led Futek to use Pressurex to help redesign several of its clamps to incorporate silicone die springs to regulate the pressure more precisely.

  • Pressurex reveals surface pressure from 2 to 43,200 psi.
  • Did you enjoy this article? Click here to subscribe to Quality Magazine. 

    You must login or register in order to post a comment.

    Multimedia

    Videos

    Podcasts

    Karen Spencer, Clinkenbeard's quality manager, discusses what makes the plant stand out, advice for other plants, and looks to the future.
    More Podcasts

    Quality Magazine

    CoverImage

    2015 May

    The May 2015 edition of Quality Magazine includes articles on cloud technologies, depth gages, ISO 9001, digital inspection and cool new products.

    Table Of Contents Subscribe

    Topics to Talk About

    What topics would you like to see Quality cover more?
    View Results Poll Archive

    Clear Seas Research

    qcast_ClearSeas_logo.gifWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

    STAY CONNECTED

    Facebook2015_40 twitter_40px.png  youtube_40px.pnglinkedin_40px.png  GooglePlus_40

    eNewsletters