Black Ox pin gages are class zz (0.0002-inch) gage pins that have a durable protective black oxide coating. The gages have clear size markings, 2-inch uniform lengths, class conformance certificates, centerless ground and a 10-microinch finish. The gages are available in complete sets or individually.