Quality Magazine

UT Supervisor Approved as NDT MIL-STD-2132 Examiner

October 15, 2009

HATFIELD, PA – Steve Walmsley, ultrasonic testing (UT) Supervisor at Laboratory Testing Inc., has been approved as an NDT MIL-STD-2132 Examiner for both immersion and contact ultrasonic testing. Walmsley completed written and operational exams on general theory, specifications and standards and ultrasonic testing methods and equipment. The examinations were administered by the Naval Sea Systems Command in Pittsburgh.

Steve Walmsley is an 18-year employee of Laboratory Testing Inc. and an NDT Level II in Ultrasonic Testing. He directs the lab’s high-speed immersion inspection for round material as narrow as 1/8 inch and as long as 75 feet, immersion UT of oversized material up to 20 feet long and a weight of 5,000 pounds., and contact inspection for other materials.

For more information, visit www.labtesting.com.