Olympus OmniScan SX Flaw Detector

September 11, 2013

OLYMPUS OMNISCAN SX FLAW DETECTORThe new OmniScan SX from Olympus is a lightweight flaw detector with an easy-to-read 8.4 in. touch screen for displaying its user-friendly and streamlined software interface. The single group OmniScan SX provides a cost-effective solution for linear zero-degree inspections, such as corrosion mapping and composite inspection, as well as weld inspection using one phased array group or one TOFD channel. 