Computed tomography inspects parts using 3-D images. • The complex geometries and miniaturization of critical components that are used by the automotive, electronics and aerospace industries require feature recognition down to the micron levels.
Middle: Microfocus X-ray image of an aluminum casting at three-fold magnification. The contrast is because of varying thickness. Note the porosities on the sample,