CEDAR PARK, TX-ASAME Technology LLC holds an exclusive license to market, distribute and support the patented Automated Surface Strain Analysis and Measurement Environment (ASAME). ASAME Technology sells and supports the ASAME Target Model and the Grid Pattern Analyzer (GPA). Currently there are more than 100 ASAME and GPA users around the world.
Scientists and engineers use the ASAME Target Model to obtain the 3-D geometry and surface strain data over critical areas of sheet metal or plastic parts efficiently and accurately. First, a grid pattern of squares or circles is applied to the surface of an undeformed sheet of metal or plastic, and the gridded blank is formed. A small photogrammetry target is placed in the view of the desired measurement area, and two or three photographs are taken of the area including the target. The ASAME software processes these images, and calculates the area's geometry and strain data. Data display features offer the capability to analyze data for specific forming applications.