CINCINNATI-ASTM E2001-8 Standard Guide for Resonant Ultrasound for Defect Detection in Both Metallic and Non-Metallic Parts has been revised and released. Standardizing resonant inspection nondestructive testing across different organizations, companies and countries for meaningful comparison and consistency is the express purpose of the new standard.