HMS Industries Inc. Selects Rize One 3D Printer to Build Functional Tooling for Production
WOBURN, MA – HMS Industries Inc., manufacturer of custom metal stamping and industrial tooling, selected the Rize One 3D printer to produce functional jigs and fixtures for holding parts in machines during CMM quality inspections.
HMS cited Rize’s zero-post-processing, isotropic part strength, ease of use and low cost for the purchase of their first 3D printer, enabling on-demand production of custom and replacement jigs and fixtures at the point of consumption in the Company’s tool and die shop.