Olympus announced the addition of a motorized steerable scanner to its line of solutions for ultrasonic and phased array testing. The field-tested, remote-controlled SteerROVER™ scanner is the most ad-vanced and versatile motorized scanner offered by Olympus. Like its forerunner the MapROVER™ scanner, the SteerROVER scanner performs circumferential weld inspection and corrosion mapping us-ing a raster arm, yet is capable of much more