ASTM International Additive Manufacturing Center of Excellence Announces First Round of R&D Projects
SINGAPORE — Global standards developer ASTM International announced its first round of funding to support research that will help catalyze the development of needed standards in additive manufacturing, also known as 3D printing.
This investment of $300,000 and in-kind contributions will help partners in the ASTM International Additive Manufacturing Center of Excellence address pressing technical information needs in this fast-growing area.