Expanding the measuring choices for die inserts used in multilayer regis-tration systems for printed circuit boards has helped reduce inspection time for Multiline Technology Inc. (Farmingdale, NY).
The design and layout of multiple layered circuit board laminations depend on a perfect die alignment, which is achieved by the company's advanced technology punch, post-etch punch and other registration equipment. To measure the accuracy of these die inserts, Multiline added new measuring equipment to the facility. One of the pieces of equipment purchased was the Trimos V-600 Height Gage supplied by Fred V. Fowler Co. (Newton, MA).