Handheld X-Ray Fluorescence (HHXRF) analyzers verify materials quickly, reliably and cost-efficiently. They can identify a material’s elemental makeup within seconds, making it easier for manufacturers to select the right metal grades and tolerances for their needs. Such precision is essential for reliable part performance, especially in aerospace, oil and gas and pharmaceutical industries.
XRF can show the user a sample’s raw material composition, which is critical, says Michel Zoontjes, product manager, Malvern Panalytical B.V.