Rapid growth in electric vehicle sales along with an increasing interest in fuel-cell-electric powertrain systems presents the auto industry with serious and largely unanticipated quality-control issues.
Billions of lithium-ion battery cells are produced annually and more than five percent are estimated to have small undetected leaks that can affect performance, shorten battery life and cause vehicle fires.