The American Welding Society will bring focus to the growing manufacturing economy of Mexico and Central America with its sponsorship of WELDMEX, May 5-7 in Monterrey, Mexico.
Weld and process monitoring is a combination of measuring and monitoring weld conditions and at the same time measuring and monitoring the additional factors that make up a quality weld.
Before the advent of the consumer GPS, a driver had the instrumentation of the car dash. While useful, it did not provide information about direction, time of travel, or time to destination.
When it comes to ensuring that defects in welds are detected in an assembly line, nondestructive testing (NDT) is an essential tool. Without a means of assessing potential errors in welds, welding would be risky business.
The WeldRover is an automated scanner for nondestructive testing (NDT) on metal plate, pipes, vessels and welded components from 4 inches in diameter to flat surfaces.