Quality Magazine logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Quality Magazine logo
  • NEWS
  • PRODUCTS
    • FEATURED PRODUCTS
    • SUBMIT YOUR PRODUCT
  • CHANNELS
    • AUTOMATION
    • MANAGEMENT
    • MEASUREMENT
    • NDT
    • QUALITY 101
    • SOFTWARE
    • TEST & INSPECTION
    • VISION & SENSORS
  • MARKETS
    • AEROSPACE
    • AUTOMOTIVE
    • ENERGY
    • GREEN MANUFACTURING
    • MEDICAL
  • MEDIA
    • A WORD ON QUALITY PUZZLE
    • EBOOKS
    • PODCASTS
    • VIDEOS
    • WEBINARS
  • EVENTS
    • EVENT CALENDAR
    • THE QUALITY SHOW
    • IMTS
  • DIRECTORIES
    • BUYERS GUIDE >
      • Supplier Insights
    • NDT SOURCEBOOK
    • VISION & SENSORS
    • TAKE A TOUR
  • INFOCENTERS
    • Digital Quality Management Systems
    • NEXT GENERATION SPC & QUALITY ANALYTICS
  • AWARDS
    • ROOKIE OF THE YEAR
    • PLANT OF THE YEAR
    • PROFESSIONAL OF THE YEAR
  • MORE
    • Expert Columns
    • NEWSLETTERS
    • QUALITY STORE
    • INDUSTRY LINKS
    • SPONSOR INSIGHTS
  • EMAG
    • eMAGAZINE
    • ARCHIVES
    • CONTACT
    • ADVERTISE
  • SIGN UP!
AutomationNDTAerospace

NDT | Aerospace

Advances in Automated NDT: Viable Inspection Solutions for Aerospace Applications

Advanced ultrasonic testing solutions must keep pace with these new challenges while maintaining the rigorous quality control standards that ensure aircraft safety.

By Ahmad Chahbaz, René Sicard
Large-scale inspection of all aircraft systems in the aircraft hangar by worker mechanics and other specialists. Bright light streaming outside from the garage door.

Image Source: aapsky / iStock / Getty Images Plus

March 2, 2025
✕
Image in modal.

Aerospace components vary in shape, size, and material composition, each requiring tailored inspection methods to ensure quality and safety. These critical parts are manufactured using diverse processes such as forging, casting, composite layups, and material bonding, each introducing unique challenges that demand specialized verification techniques. Despite these variations, all aerospace components must undergo rigorous inspections to meet stringent industry standards.

Automated Ultrasonic Testing (UT) systems play a key role in improving efficiency, reducing inspection time, and enhancing imaging and defect detection capabilities. However, to fully harness the potential of automated ultrasonic testing solutions, advanced tools are essential at multiple levels: scanner control, inspection planning, and UT results analysis.

THE NEED FOR ADVANCED TOOLS IN AUTOMATED UT INSPECTION

By integrating advanced tools at every stage of the UT inspection process (scanner control, inspection planning, and results interpretation), automated NDT systems can deliver the precision, efficiency, and reliability required for modern aerospace manufacturing.

Figure 1. Gantry system with 3D and contour following scanning capabilities
Figure 1. Gantry system with 3D and contour following scanning capabilities Image Source: TecScan

Scanner Control Tools

Ultrasonic testing of aerospace components with complex 3D geometries requires advanced control tools to achieve precise and comprehensive scanner control. For example, UT immersion tanks and squirter gantry systems integrate contour-following capabilities and multi-axis motion control to ensure accurate UT inspection coverage. These systems can also be equipped with 3D Scanning capabilities using advanced path-planning algorithms to adapt to intricate surface profiles, enabling full volumetric inspection. Additional scanner control capabilities and tools are also required to monitor and maintain the ultrasonic probes alignment to achieve proper scanning resolutions. 

Inspection Planning Tools

In the scanner control software environment, inspectors need intuitive inspection and planning tools to allow them to define the UT scan paths easily and with precision. This can be done by creating a realistic and accurate virtual CAD representation of both the part and the scanner within the software control environment. Operators can also use such tool to calibrate the scanner and simulate the whole UT inspection process.

Figure 2. TecView virtual environment with CAD models of an immersion tank and the inspected part
Figure 2. TecView virtual environment with CAD models of an immersion tank and the inspected part Image Source: TecScan

This virtual 3D display environment can also be used to assist with the preparation of scanning paths, more specifically to modify scanning path to avoid areas where mechanical limitations are reached and collisions become inevitable, as well as in the definition of safe probe approach trajectories. These inspection tools not only streamline the scan preparation process but can also enhance repeatability and reliability in UT testing.

NDT Analysis Tools

Finally, the accuracy of any nondestructive testing (NDT) solution relies on robust results interpretation tools. Advanced data processing software must be capable of analyzing vast amounts of inspection data, filtering out noise, and highlighting potential defects with high precision. Intelligent algorithms, 3D visualization, and user-driven analysis further improve defect detection, ensuring reliable results that meet aerospace quality standards.

A key example of such analysis tools is the gain correction map algorithm, which allows us to account for natural signal attenuation in complex geometries by dynamically adjusting the receiver gain as the probe(s) move across the surface of the inspected part or component. This is based on a pre-calibration of the attenuation occurring naturally on the part.

Figure 3. C-Scan results of composite structure with Gain Correction Map
Figure 3. C-Scan results of composite structure with Gain Correction Map Image Source: TecScan

Variable signal gating is another essential tool, particularly when variations in component thickness prevents from using simple gates to detect indications without interferences from the back wall echo. With position-dependent gating, the detection gate dynamically adjusts based on the B-Scan representation, following the component thickness.

Figure 4. Examples of variable inspection gating using TecView for composite U-Shape and Strake parts
Figure 4. Examples of variable inspection gating using TecView for composite U-Shape and Strake parts Image Source: TecScan

Other advanced tools and analysis capabilities include automatic detection of indications from the C-Scan data, creating lists of indications after separation and merging of pixels based on user-defined criteria, various signal-to-noise analysis types (statistical or local), and advanced reporting tools.

SELECTED APPLICATIONS FOR AUTOMATED TESTING OF AIRCRAFT COMPONENTS

Composite materials are now widely used for a variety of aircrafts parts, from honeycomb sandwiched structures found in wing flaps to 3D woven composite materials such as the LEAP engine fan blades. Most composite materials can be considered as 3D panels, meaning they have curved surfaces with mostly parallel planes. Both pulse-echo and transmission scans are used on such parts depending on the type of defects to be detected. While porosity is typically characterized by attenuation of the backwall echo in a pulse-echo setup, bonding quality is often assessed by transmitting ultrasounds through the part’s thickness. In honeycomb structures, transmission is the only viable option since backwall echoes rarely propagate back through the core.

The following sections highlight key applications of automated testing systems equipped with advanced NDT scanning tools.

U-Shaped Carbon Composite Part

This example highlights advanced motion control and data interpretation functionalities necessary to fulfill inspection requirements. The U-shaped carbon composite part features areas of different thicknesses. Despite its simple appearance, 3D contour following scanning is required to maintain a constant beam entry angle and water path. Variable gating is also necessary to avoid setting up a specific gate for each thickness variation.

Figure 5. Automated immersion system used for the inspection of U-Shaped carbon composite panel
Figure 5. Automated immersion system used for the inspection of U-Shaped carbon composite panel Image Source: TecScan

Since porosity is often monitored in carbon composite laminates, backwall echoes attenuation must be analyzed. This can be done by evaluating the acceptable dB drop for each thickness range or calculating the attenuation per units of thickness.

Figure 6. Different C-Scan representations resulting from the inspection of the U-Shaped carbon composite panel. C-Scan 1 (top-left) and C-Scan 2 (top-right) illustrate the benefit of using variable gate
Figure 6. Different C-Scan representations resulting from the inspection of the U-Shaped carbon composite panel. C-Scan 1 (top-left) and C-Scan 2 (top-right) illustrate the benefit of using variable gate Image Source: TecScan

In the above example of Fig. 6, the benefits of variable gating (C-Scan 2, top-right) for the detection of internal indications is illustrated by comparison to a fixed gate (C-Scan 1, top-left). Porosity characterization can also benefit from a conversion of backwall amplitude (C-Scan 3, bottom-left) to attenuation data (C-Scan 4, bottom-right). While direct backwall amplitude must be compared to the expected signal amplitude or drop corresponding to the thickness of a specific area, attenuation provides a reading that is independent from thickness. This is beautifully illustrated in this example, where large variations observed on the backwall amplitude are not relevant when converted to attenuation, especially for the lowest monitored backwall amplitude which converts to the lowest attenuation.

To enhance data reporting efficiency, C-Scan images can be projected onto the actual 3D shape of the inspected part, improving both the positioning and visualization of detected indications.

Figure 7. Projecting the C-Scan images on the 3D shape of the part helps with the visualization of the indications within the parts
Figure 7. Projecting the C-Scan images on the 3D shape of the part helps with the visualization of the indications within the parts Image Source: TecScan

Aircraft Wing Flaps

Aircraft wing flaps represent another example of 3D composite panels requiring advanced tools to obtain optimal scan results. The sample presented below is an aluminum honeycomb core bonded to curved aluminum skins, scanned in a through-transmission setup using a pair of phased array probes.

Due to its curved shape, 3D contour following is necessary. However, the presence of the honeycomb structure complicates the scanning trajectories calculation. As an example, the general cross-sectional shape of a wing flap is presented in Fig. 8; as illustrated by the parallel lines, the honeycomb cell walls run through the thickness independently from the angle of the skin surface. In addition, the thickness of the honeycomb structure varies along the part profile, leading to variations of ultrasonic attenuation.

Ultrasonic waves can only propagate through the walls of the honeycomb cells, which means that the emitting and receiving probes locates on both sides of the sample must align with the cell’s walls to get proper transmission through the thickness. Consequently, the motion control software must allow to associate entry and exit points that are aligned with the core cells in the calculation of scanning trajectories. Phased array scanning is also beneficial to minimize scanning time on such large structures. This requires state-of-the art algorithms to manage data acquisition of phased array on curved surfaces that preserves the true dimensions of the part.

Figure 8. Cross-section of a wing flap illustrating the variations of honeycomb cell walls vs skin layers
Figure 8. Cross-section of a wing flap illustrating the variations of honeycomb cell walls vs skin layers Image Source: TecScan

Since the thickness of the honeycomb structure is not the same everywhere and the direction of propagation of ultrasounds inside the part is not necessarily achieved with optimal entry and exit angle at the skin surface, significant differences in wave attenuation can occur across the part. A gain correction map function that dynamically corrects the gain as a function of local attenuation represents a highly valuable tool for such structure. By correcting the gain as a function of scanning position, a strong signal can be maintained across the part, leading to the same amplitude accuracy and an optimal signal-to-noise ratio at any position. Benefits of this technique are illustrated in the C-Scan images of Fig. 9, which were acquired on a wing flap sample, both without and with the gain correction map.

Figure 9. Comparison of pre and post application of the Gain Correction Map on an aircraft wing flap in TecView
Figure 9. Comparison of pre and post application of the Gain Correction Map on an aircraft wing flap in TecView Image Source: TecScan

Aircraft Engine Nacelle Chines and Strakes

Aircraft engine chines and strakes represent a slightly more complex form of composite panels. With their T-shape, multiple setups are required to scan the entire part. In the example below, the fin of a strake was scanned in a through-transmission setup, while both sides of the flange are scanned in pulse-echo. These scans were done using a 10-axis scanner with two independent sets of X-Y-Z-A-B axes.

One of the tools that can minimize scan time is a batch scan utility, i.e. the ability to execute multiple scan setups automatically without requiring any operator intervention. Pulse-echo and through-transmission scans were therefore performed in a programmed sequence, as illustrated in Fig. 10. In addition, these structures have varying thickness that require variable gating for pulse-echo scan data interpretation.

Figure 10. 3D representation of Pulse-Echo and Transmission scans in an engine strake obtained by running a sequence of inspection setups
Figure 10. 3D representation of Pulse-Echo and Transmission scans in an engine strake obtained by running a sequence of inspection setups Image Source: TecScan

Another particularity of the strakes and chines is the tight radius of the transition between the fin and the flange. Scanning surfaces at and around the flange radius therefore presents high risks of interference between the probe gimbal manipulator and the part.

Figure 11. Example of identification of collision in TecView 3D display environment from the intersection of the scanner model with the inspected part model
Figure 11. Example of identification of collision in TecView 3D display environment from the intersection of the scanner model with the inspected part model Image Source: TecScan

This is where accurate simulation tools become essential in the preparation of the scan setup. Collisions can be identified by simulating the movement of the probe around the radius at the required water column and angle and trajectories can be modified to avoid such interferences. This exercise leads to an optimization of the scanning time by maximizing areas of the part that can be scanned automatically, while identifying areas where a complementary manual inspection may be necessary. In the example below, a section of surface identified by simulation and leading to collisions has been removed from the scanning area, thus avoiding the problematic trajectories.

Fig. 12. Display of the inspection area after removal of the scanning positions responsible for mechanical interference illustrated in Fig. 10.
Fig. 12. Display of the inspection area after removal of the scanning positions responsible for mechanical interference illustrated in Fig. 10. Image Source: TecScan
Figure 13. Pulse-Echo C-Scan resulting from the inspection of the strake sample after removal of the problematic scanning positions.
Figure 13. Pulse-Echo C-Scan resulting from the inspection of the strake sample after removal of the problematic scanning positions. Image Source: TecScan

Conclusions

Multiple advanced ultrasonic scanning tools were highlighted through examples of scan data acquired on various aircraft components. While 3D contour-following scanning tools were featured in all presented cases, additional valuables functions, such as the scanner’s virtual 3D environment display and offline simulation, were demonstrated for engine carbon composite strakes and chines. These part, with small flange radii, pose a high risk of mechanical interferences with the automated probe holder gimbal head. By simulating the scanning environment, potential collisions were identified, allowing problematic scanning coordinates to be excluded from the scanning trajectories. This case exemplifies optimal inspection setup planning, where automated ultrasonic scanning coverage is maximized, leaving only a minimal area for manual inspection. The advantages of batch scanning were also highlighted in this example, as downtime was reduced by minimizing operator intervention between scans of different areas of the part.

The importance of defining 3D scanning trajectories based on ultrasonic wave propagation paths was discussed, particularly in cases such as aircraft wing flaps. Since ultrasonic propagation within honeycomb structures is constrained by the cell walls, scanning trajectories must be defined accordingly rather than relying solely on geometrical considerations such as the midplane or the angles of external surfaces.

Various data interpretation and analysis tools were also presented, starting with variable scanning gates. As demonstrated in the examples of carbon composite U-shaped and strake structures, this tool is essential for analyzing composite panels with varying thicknesses. Additionally, the gain correction mapping algorithm was illustrated using an aircraft wing flap as an example. By referencing pre-calibrated attenuation measurements from a known good part, this tool dynamically adjusts the receiver gain for each scanned point, simplifying data interpretation. This was particularly beneficial for the wing flap, where variations in honeycomb thickness resulted in significant differences in ultrasonic wave attenuation. Applying the gain correction map ensured a more uniform response across the scanned surface.

As aerospace components continue to evolve with increasing reliance on composite materials, advanced ultrasonic testing solutions must keep pace with these new challenges while maintaining the rigorous quality control standards that ensure aircraft safety.

READ MORE

  • Flaw Detection in Aircraft Engine Fan Components using Automated Ultrasonic Technologies
  • Advanced Eddy Current Scanning Solution for Aero Engine High Pressure Compressor Rotor Spools
  • Automated Eddy Current Testing Solution for Aero-engine Discs
KEYWORDS: analysis manufacturing metrology ultrasonic testing (UT) ultrasonics

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Ahmad Chahbaz is the CEO of TecScan Systems. For more information, email [email protected] or visit www.tecscan.ca.

René Sicard is the R&D manager of TecScan Systems Inc. (Boucherville, Quebec, Canada). For more information, call (450) 641-5876, e-mail [email protected] or visit www.tecscan.ca.

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • 2024 Quality Rookie of the Year Justin Wise 1440x750px banner with "Quality Rookie of the Year" logo inset

    Meet the 2024 Quality Rookie of the Year: Justin Wise

    Justin Wise is an exceptional individual who has been...
    Aerospace
    By: Michelle Bangert
  • Man with umbrella and coat stands outside while it rains at night looking at a building.

    Nondestructive Testing: Is there an ethics problem?

    I was a whistleblower who exposed fraudulent activities...
    NDT
    By: Dale Norwood
  • Unraveling Deflategate: Football stadium with closeup of football on field

    Unraveling the Tom Brady Deflategate

    The Deflategate scandal erupted following the 2014 AFC...
    Measurement
    By: Greg Cenker and Henry Zumbrun
Manage My Account
  • eMagazine Subscriptions
  • Newsletters
  • Online Registration
  • Subscription Customer Service
  • Manage My Preferences

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Quality audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Quality or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Key Takeaways for Quality Leaders
    Sponsored byComplianceQuest

    Key Takeaways for Quality Leaders from the 2026 Gartner Magic Quadrant™ for QMS

  • This image shows a person seated next to a Bobcat T66 compact track loader.
    Sponsored byPolyWorks by InnovMetric

    Supercharging Digital Gauging at Bobcat North America

  • Dorsey Calibration Lab photo by Tom LaBarbera Picture this Studios
    Sponsored byDorsey Metrology International

    Ensuring Product Quality in a Competitive Manufacturing Landscape

Popular Stories

Visions Sensors Ebook

eBook | How AI-driven Vision Systems Are Transforming Automotive Quality Control

Person reviewing analytics dashboards on multiple computer monitors.

Preparing for the Transition to ISO 14001:2026

Emily_Q-Cast_Image.jpg

More on That One Thing Elon Gets Right

2026 Quality Professional of the Year!

Events

July 14, 2026

Quality Leaders Forum: Better Communication, Better Quality Data

The Quality Leaders Forum is a quarterly, editor-moderated fireside chat series hosted by Quality Magazine, featuring candid conversations with senior manufacturing and operations executives shaping enterprise-level quality.

August 12, 2026

Eliminate Manual FAI Processes and Reduce Inspection Time by Up to 90%

Discover how advanced FAI software automates First Article Inspection workflows by generating inspection plans, validating results in real time, integrating 2D/3D data, and reducing quality escapes to improve efficiency and compliance.

View All Submit An Event

Products

Lean Manufacturing and Service Fundamentals, Applications, and Case Studies

Lean Manufacturing and Service Fundamentals, Applications, and Case Studies

See More Products
Rookie of the Year Custom Content

Related Articles

  • Fig. 1: Raster scan using Single element UT vs Phased Array.

    Enhancing Automated NDT: Leveraging Advanced 3D Phased Array Scanning and C-Scan Mapping Techniques for Aerospace Applications

    See More
  • 01 QM 0823 Test and Inspection B Strain Gauge

    Important Considerations for Tensile Testing Equipment in Aerospace Applications

    See More

Related Products

See More Products
  • Factory Physics for Managers: How Leaders Improve Performance in a Post-Lean Six Sigma World

  • lean manu.jpg

    Lean Manufacturing and Service Fundamentals, Applications, and Case Studies

See More Products

Related Directories

  • NDT Solutions LLC

    NDT Solutions (ndts.com) is a leader in digital Nondestructive Testing, delivering advanced NDI systems, calibration, consulting, and SME support. We provide lab and field services, R&D, engineering, and “Lab-in-a-Box” solutions, including the AUSS and MAUS systems, transforming inspection through innovation and tailored deployment.
  • TecScan Systems Inc.

    TecScan manufactures advanced Automated Non-Destructive Testing (NDT) systems for aerospace, power generation, and manufacturing industries. We specialize in automated ultrasonic testing, including ultrasonic immersion tanks, phased array inspection systems, gantry-based NDT systems, and automated eddy current testing systems. Our portfolio also includes manual and automated portable scanners engineered for precision inspection and quality assurance.
×

Stay in the know with Quality’s comprehensive coverage of
the manufacturing and metrology industries.

Newsletters | Website | eMagazine

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Market Research
    • Reprints
    • List Rental
    • Survey/Respondent Access
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • YouTube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing